Causes of surface crack of aluminum profile

  • 2019-12-03
  • 1555

(I): the extrusion coefficient of aluminum profile is too large, the extrusion temperature is too high (three temperatures of bar, barrel and die), and the extrusion speed is too fast.

(II): the extrusion pressure is unstable, high and low, or the speed difference between multi speed regulation is obvious, and the speed conversion is sudden fast when shifting.

(3): when extruding aluminum alloy profiles, the head end pressing (Stamping) is too fast, the tail end running speed or not slowing down, and a large amount of dead zone aluminum infiltrates.

(IV): the quality of the rod is poor, the rod is overburned, with large grains and loose. The residual pressure (V3 aluminum) is too thin.

(V): the design and manufacture of the extrusion die with the velocity ratio seriously misaligned is unreasonable.


PRODUCT RECOMMENDATIONS

ONLINE MESSAGE

If you are interested in our products, or what we can do to help you, you can call our national service number at any time:13512567272(Mr. Shi) You can also communicate with us online, of course, you can also leave us a message below, we will serve you warmly!

安吉县| 日土县| 溧水县| 万荣县| 剑川县| 鄱阳县| 布尔津县| 新闻| 昭苏县| 清丰县| 克什克腾旗| 泰州市| 那曲县| 庐江县| 罗城| 汝南县| 平凉市| 中牟县| 邮箱| 封丘县| 两当县| 扶余县| 鹤山市| 深泽县| 黄浦区| 铜梁县| 都兰县| 北京市| 嘉善县| 南雄市| 佛冈县| 华阴市| 台南市| 江阴市| 南城县| 乐昌市| 江川县| 杂多县| 昌平区| 遵化市| 康保县|